Polymer Property : Charpy Impact Unnotched = 6.50 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 1.39 - 6.50 J/cm²

@Temperature -40.0 - 30.0 °C
6.62 - 30.9 ft-lb/in²

@Temperature -40.0 - 86.0 °F
Average value: 3.68 J/cm² Grade Count:66
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..
Charpy Impact Unnotched 4.50 - 6.50 J/cm²

@Temperature -30.0 - -20.0 °C
21.4 - 30.9 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 5.70 J/cm² Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35..
Charpy Impact Unnotched 2.00 - 6.50 J/cm²

@Temperature -30.0 - -30.0 °C
9.52 - 30.9 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.16 J/cm² Grade Count:14
Overview of materials for PBT + ASA Blend, Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PBT + ASA Blend, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum ..
Charpy Impact Unnotched 2.00 - 6.50 J/cm²
9.52 - 30.9 ft-lb/in²
Average value: 4.05 J/cm² Grade Count:12
Overview of materials for Nylon 66, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of ..
Charpy Impact Unnotched 2.60 - 6.50 J/cm²
12.4 - 30.9 ft-lb/in²
Average value: 4.16 J/cm² Grade Count:20
Overview of materials for Nylon 66, Carbon Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Carbon Fiber/PTFE Filled". Each property range of values reported is minimum and maximum value..
Charpy Impact Unnotched 4.00 - 6.50 J/cm²
19.0 - 30.9 ft-lb/in²
Average value: 5.23 J/cm² Grade Count:10
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..
Charpy Impact Unnotched 3.00 - 6.50 J/cm²
14.3 - 30.9 ft-lb/in²
Average value: 5.33 J/cm² Grade Count:3
Overview of materials for Nylon 66, Glass Fiber/MoS2 Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/MoS2 Filled". Each property range of values reported is minimum and maximum values..
Charpy Impact Unnotched 2.10 - 6.50 J/cm²
9.99 - 30.9 ft-lb/in²
Average value: 4.59 J/cm² Grade Count:15
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% ..
Charpy Impact Unnotched 2.40 - 6.50 J/cm²
11.4 - 30.9 ft-lb/in²
Average value: 5.20 J/cm² Grade Count:7
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..
Charpy Impact Unnotched 2.10 - 6.50 J/cm²

@Temperature -30.0 - -30.0 °C
9.99 - 30.9 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 4.62 J/cm² Grade Count:6
Overview of materials for Polyethylene Terephthalate (PET), 50% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 50% Glass Reinforced". Specific grades with glass content between 45% ..