Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 6.80 J/cm² | 32.4 ft-lb/in² | ISO 179/1eU |
Radici Radilon® CARV300 L (dry) Copolyamide 66/6 Glass-fiber reinforcedInformation provided by Radici group. |
|||
Charpy Impact Unnotched | 6.80 J/cm² @Temperature -30.0 °C |
32.4 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Lehmann & Voss LUVOCOM® 20-0778 Polyphthalamide, with glass fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an.. |
|||
Charpy Impact Unnotched | 6.80 J/cm² | 32.4 ft-lb/in² | |
Idemitsu Kosan Xarec® N WA 7030 SPS, 30% Glass Filled Crystalline Polymer Blend, Glass Filled, Impact Modified |
|||
Charpy Impact Unnotched | 6.80 J/cm² @Temperature 23.0 °C |
32.4 ft-lb/in² @Temperature 73.4 °F |
ISO 179-1eU |
Gromax BFG30-DN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Charpy Impact Unnotched | 6.80 J/cm² | 32.4 ft-lb/in² | edgewise; ISO 179 1eU |
Lehmann & Voss LUVOCOM® 1105/XCF/15-S PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at.. |
|||
Charpy Impact Unnotched | 6.80 J/cm² | 32.4 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 218G1 V25 Black 34N PA66, 25% glass fiber, DRY Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail.. |
|||
Charpy Impact Unnotched | 6.80 J/cm² | 32.4 ft-lb/in² | ISO 179/1eU |
Solvay TECHNYL® A 548B V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B V15 is a copolyamide 6.6/6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits:.. |