Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Crush Resistance | 11300 kg | 25000 lb (mass) | Compressive Strength |
Glastic Laminates/Shapes 1872 Fiberglass-Reinforced Polyester Standoff Insulator Data provided by Glastic Corporation.Molded from UL recognized molding compound. Moisture and heat resistance of Glastic Insulators are higher than those of conventional plastic insulators. |
|||
Crush Resistance | 11300 kg | 25000 lb (mass) | Compressive Strength |
Glastic Laminates/Shapes 2035-1 Fiberglass-Reinforced Polyester Standoff Insulator Data provided by Glastic Corporation.Molded from UL recognized molding compound. Moisture and heat resistance of Glastic Insulators are higher than those of conventional plastic insulators. |