Mechanical Properties Metric English Comments
Crush Resistance 11300 kg
25000 lb (mass)
Compressive Strength
Glastic Laminates/Shapes 1872 Fiberglass-Reinforced Polyester Standoff Insulator
Data provided by Glastic Corporation.Molded from UL recognized molding compound. Moisture and heat resistance of Glastic Insulators are higher than those of conventional plastic insulators.
Crush Resistance 11300 kg
25000 lb (mass)
Compressive Strength
Glastic Laminates/Shapes 2035-1 Fiberglass-Reinforced Polyester Standoff Insulator
Data provided by Glastic Corporation.Molded from UL recognized molding compound. Moisture and heat resistance of Glastic Insulators are higher than those of conventional plastic insulators.