Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Creep Strength | 35.0 MPa @Temperature 150 °C, Time 720000 sec |
5080 psi @Temperature 302 °F, Time 200 hour |
0.2% strain |
AMT AM-Lite® Die Casting Magnesium Alloy AM-lite is a high surface finish die casting alloy suitable for applications that currently utilize zinc, aluminum or magnesium (alloy AZ91D) die castings, or plastic injection moldings. AM-lite has.. |
|||
Creep Strength | 35.0 MPa @Time 360000 sec |
5080 psi @Time 100 hour |
in water at 95°C |
BASF Ultrason® P 3010 PPSU Unreinforced Polyphenylsulfone Description: Medium viscosity injection-molding and extrusion grade with good toughness and chemical resistance (stress crack resistance), resistant against superheated steam. The property profile m.. |