Polymer Property : Izod Impact Notched = 0.970 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact Notched 1.32 J
0.970 ft-lb
ASTM D256A
ExxonMobil PP4712E1 Polymer Grade for Oriented Film
Product Description: Easy processing grade primarily for oriented film applications.Availability: North America and South America Features:MetalizableUses: Industrial Applications Oriented FilmTo..