Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact Notched | 1.32 J | 0.970 ft-lb | ASTM D256A |
ExxonMobil PP4712E1 Polymer Grade for Oriented Film Product Description: Easy processing grade primarily for oriented film applications.Availability: North America and South America Features:MetalizableUses: Industrial Applications Oriented FilmTo.. |