Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.270 J/cm | 0.506 ft-lb/in | ASTM D256 |
North Wood Plastics HDPE with 60% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Izod Impact, Unnotched | 0.270 - 2.40 J/cm | 0.506 - 4.50 ft-lb/in | Average value: 1.11 J/cm Grade Count:5 |
Overview of materials for High Density Polyethylene (HDPE), Wood Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Wood Filled". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Unnotched | 0.270 J/cm @Temperature -40.0 °C |
0.506 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, 50% RH Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by Gehri.. |