Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.270 J/cm
0.506 ft-lb/in
ASTM D256
North Wood Plastics HDPE with 60% Wood Fiber
Data provided by North Wood Plastics, Inc.
Izod Impact, Unnotched 0.270 - 2.40 J/cm
0.506 - 4.50 ft-lb/in
Average value: 1.11 J/cm Grade Count:5
Overview of materials for High Density Polyethylene (HDPE), Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Wood Filled". Each property range of values reported is minimum and ma..
Izod Impact, Unnotched 0.270 J/cm

@Temperature -40.0 °C
0.506 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Aardvark Polymers Aarlon® 2000 Rotational Molding Resin, 50% RH
Aarlon® 2000 PA 6/6 is a high performance nylon for rotational molding applications. Aarlon® 2000 offers high heat capabilities with exceptional mechanical properties.Information provided by Gehri..