Izod Impact, Unnotched 0.392266 - 2.54973 J/cm

@Temperature -30.0 - -20.0 °C
0.734875 - 4.77669 ft-lb/in

@Temperature -22.0 - -4.00 °F
Average value: 0.848 J/cm Grade Count:27
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..
Izod Impact, Unnotched 0.392266 - 2.54973 J/cm

@Thickness 3.20 - 6.40 mm
0.734875 - 4.77669 ft-lb/in

@Thickness 0.126 - 0.252 in
Average value: 0.848 J/cm Grade Count:27
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma..