Polymer Property : Izod Impact, Unnotched = 0.680 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.680 J/cm
1.27 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON MX01739C PP
LNP* SAT-KON* MX01739C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System.