Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.680 J/cm | 1.27 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON MX01739C PP LNP* SAT-KON* MX01739C is a compound based on Polypropylene containing Proprietary Filler(s). Added features of this grade include: Electrically Conductive, Clean Compounding System. |