Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.480 J/cm - NB
0.899 ft-lb/in - NB
Average value: 7.02 J/cm Grade Count:48
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Izod Impact, Unnotched 0.480 J/cm
0.899 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer
LNP* LUBRICOMP* KG002 is a compound based on Acetal Copolymer resin containing 10% Graphite. Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched 0.480 J/cm
0.899 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP KG002 Acetal Copolymer (Asia Pacific)
LNP* Lubricomp* KG002 is a compound based on Acetal Copolymer resin containing Graphite Powder. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Ensinger TECAPRO™ MT Medical Grade Polypropylene (PP)
TECAPRO™ MT is an FDA approved homopolymer polypropylene based material with exceptionally low residual stress to facilitate the fabrication of dimensionally stable parts with varying cross section..