Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS LNP THERMOCOMP* AH0230A is a compound based on ABS resin. Added feature of this material is: High Specific Gravity. |
|||
Izod Impact, Unnotched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS (Asia Pacific) LNP THERMOCOMP* AH0230A is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Unnotched | 0.900 J/cm | 1.69 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP AH0230A ABS (Europe-Africa-Middle East) LNP THERMOCOMP* AH0230A is a compound based on Acrylonitrile Butadiene Styrene resin. Added features of this material include: High Specific Gravity. |
|||
Izod Impact, Unnotched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp OF002A PPS LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 0.900 J/cm @Temperature 23.0 °C |
1.69 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp OF002A PPS (Asia Pacific) LNP* Thermocomp* OF002A is a compound based on Polyphenylene Sulfide resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 0.900 - 1.60 J/cm | 1.69 - 3.00 ft-lb/in | Notch Status Unknown |
Goodfellow Nickel 70/Copper 30 Alloy Information provided by Goodfellow. |