Goodfellow Nickel 70/Copper 30 Alloy

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Goodfellow
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Goodfellow Nickel 70/Copper 30 Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Goodfellow.
Physical Properties Metric English Comments
Density 8.90 g/cc
0.322 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell 100 - 260
100 - 260
Tensile Strength at Break 480 - 1200 MPa
69600 - 174000 psi
Elongation at Break <= 50 %
<= 50 %
Tensile Modulus 160 - 180 GPa
23200 - 26100 ksi
Izod Impact, Unnotched 0.900 - 1.60 J/cm
1.69 - 3.00 ft-lb/in
Notch Status Unknown
Thermal Properties Metric English Comments
CTE, linear 13.6 - 14.0 µm/m-°C

@Temperature 20.0 - 100 °C
7.56 - 7.78 µin/in-°F

@Temperature 68.0 - 212 °F
Thermal Conductivity 26.0 W/m-K
180 BTU-in/hr-ft²-°F
Melting Point 1300 - 1350 °C
2370 - 2460 °F
Solidus 1300 °C
2370 °F
Liquidus 1350 °C
2460 °F
Component Elements Properties Metric English Comments
Copper, Cu 30 %
30 %
Nickel, Ni 70 %
70 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000480 ohm-cm
0.0000480 ohm-cm