Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.47 J/cm | 2.76 ft-lb/in | ASTM D256 |
Hyosung Topilene B201Y PP B201Y Extrusion Special Purpose GradeApplications:Thermoforming sheetExtrusion blow moldingCharacteristics:Low smellFormabilityInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 1.47 J/cm | 2.76 ft-lb/in | ASTM D256 |
Hyosung Topilene J340 PP J340 Injection Impact CopolymerApplications:CrateContainerBatter caseCharacteristics:High ImpactInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 1.47 J/cm | 2.76 ft-lb/in | ASTM D256 |
Hyosung Topilene J340E PP J340E Impact CopolymerApplications:Corrugated sheetThick board (tank, etc…)Characteristics:High impactHigh stiffnessLow warpageInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 1.47 J/cm @Temperature 23.0 °C |
2.75 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp OB008 PPS - Branched LNP* Thermocomp* OB008 is a compound based on Branched PPS containing Glass Beads.This data was supplied by SABIC-IP for the Americas region. |