Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hyosung Topilene B201Y PP

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Hyosung Co.
Trade Name Topilene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hyosung Topilene B201Y PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
B201Y Extrusion Special Purpose GradeApplications:Thermoforming sheetExtrusion blow moldingCharacteristics:Low smellFormabilityInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 0.50 g/10 min
0.50 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Yield 35.3 MPa
5120 psi
ASTM D638
Elongation at Break 500 %
500 %
ASTM D638
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Izod Impact, Unnotched 1.47 J/cm
2.76 ft-lb/in
ASTM D256
0.294 J/cm

@Temperature -10.0 °C
0.551 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
ASTM D648
Vicat Softening Point 145 °C
293 °F
ASTM D1525
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved