Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.54 J/cm

@Thickness 6.40 mm
2.89 ft-lb/in

@Thickness 0.252 in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC1010 PPE+HIPS (Europe-Africa-Middle East)
LNP* Stat-kon* Noryl_FMC1010 compound is a 10% carbon fiber, static dissipative, foamable resin Nonchlorinated, nonbrominated. UL94 V1 rated. Property values at 20% WR, 0.250"" wall.
Izod Impact, Unnotched 1.54 J/cm

@Thickness 6.40 mm
2.89 ft-lb/in

@Thickness 0.252 in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC1010 PPE+PS
LNP* Stat-kon* Noryl_FMC1010 compound is a 10% carbon fiber, static dissipative, foamable resin Nonchlorinated, nonbrominated. UL94 V1 rated. Property values at 20% WR, 0.250"" wall.