Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.54 J/cm @Thickness 6.40 mm |
2.89 ft-lb/in @Thickness 0.252 in |
ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC1010 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_FMC1010 compound is a 10% carbon fiber, static dissipative, foamable resin Nonchlorinated, nonbrominated. UL94 V1 rated. Property values at 20% WR, 0.250"" wall. |
|||
Izod Impact, Unnotched | 1.54 J/cm @Thickness 6.40 mm |
2.89 ft-lb/in @Thickness 0.252 in |
ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON Noryl_FMC1010 PPE+PS LNP* Stat-kon* Noryl_FMC1010 compound is a 10% carbon fiber, static dissipative, foamable resin Nonchlorinated, nonbrominated. UL94 V1 rated. Property values at 20% WR, 0.250"" wall. |