Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.39 J/cm | 10.1 ft-lb/in | ASTM D256 |
Hyosung Topilene HB240P PP HB240P Applications:Industrial pipesSewerage pipesCharacteristics:High impact strengthHigh ring stiffnessInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 5.39 J/cm | 10.1 ft-lb/in | ASTM D256 |
Hyosung Topilene HB242P PP HB242P Applications:Industrial pipesSewerage pipesCharacteristics:High impact strengthHigh ring stiffnessInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 5.39 J/cm @Temperature 23.0 °C |
10.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp EL004 PEI LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Americas.. |
|||
Izod Impact, Unnotched | 5.39 J/cm @Temperature 23.0 °C |
10.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp EL004 PEI (Asia Pacific) LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Izod Impact, Unnotched | 5.38 J/cm | 10.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP JFL34 PES LNP* LUBRICOMP* JFL34 is a compound based on Polyethersulfone resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched | 5.37 J/cm | 10.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP KFI15 ACETAL LNP* LUBRICOMP* KFI15 is a compound based on Acetal containing 25% Glass Fiber, 2% Silicone. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched | 5.41 J/cm | 10.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON FX98501 PE LNP* STAT-KON* FX98501 is a compound based on Polyethylene resin containing Proprietary Fillers. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched | 5.39 J/cm @Temperature 23.0 °C |
10.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 5.39 J/cm @Temperature 23.0 °C |
10.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA (Asia Pacific) LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched | 5.39 J/cm | 10.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer LNP THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing 20% Milled Glass. |
|||
Izod Impact, Unnotched | 5.39 J/cm | 10.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer (Asia Pacific) LNP* THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass. |
|||
Izod Impact, Unnotched | 5.39 J/cm | 10.1 ft-lb/in | ASTM Data |
Dow Retain® 8209 ABS + Polycarbonate Data provided by Dow Chemical. |
|||
Izod Impact, Unnotched | 5.40 J/cm | 10.1 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy E-13370B Internally Lubricated, Glass Fiber Reinforced Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Izod Impact, Unnotched | 5.40 J/cm | 10.1 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy E-16822-1B Internally Lubricated, Carbon Fiber Reinforced Nylon 6/6 Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Izod Impact, Unnotched | 5.39 J/cm | 10.1 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Lubrilon® 640 Nylon 6/12, PTFE Reinforced, Flow Enhanced Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |