Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.40 J/cm | 10.1 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy E-13370B Internally Lubricated, Glass Fiber Reinforced Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Izod Impact, Unnotched | 5.40 J/cm | 10.1 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy E-16822-1B Internally Lubricated, Carbon Fiber Reinforced Nylon 6/6 Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |