Izod Impact, Unnotched 10.35 J/cm
19.39 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP UFL36S PPA
LNP LUBRICOMP* UFL36S is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant, Bearing Grade.
Izod Impact, Unnotched 10.35 J/cm
19.39 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP UFL36SXP PPA
LNP LUBRICOMP* UFL36SXP is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant.