Material Notes:
LNP LUBRICOMP* UFL36SXP is a compound based on Polyphthalamide resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant.
Physical Properties Metric English Comments
Density 1.55 g/cc
0.0560 lb/in³
ASTM D792
1.55 g/cc
0.0560 lb/in³
ISO 1183
Moisture Absorption 0.330 %
0.330 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0017 cm/cm

@Time 86400 sec
0.0017 in/in

@Time 24.0 hour
ISO 294
0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm

@Time 86400 sec
0.0080 in/in

@Time 24.0 hour
ASTM D955
0.0082 cm/cm

@Time 86400 sec
0.0082 in/in

@Time 24.0 hour
ISO 294
Mechanical Properties Metric English Comments
Tensile Strength at Break 196 MPa
28400 psi
ASTM D638
196 MPa
28400 psi
ISO 527
Elongation at Break 2.5 %
2.5 %
ASTM D638
2.5 %
2.5 %
ISO 527
Tensile Modulus 9.88 GPa
1430 ksi
1 mm/min; ISO 527
12.41 GPa
1800 ksi
50 mm/min; ASTM D638
Flexural Strength 280 MPa
40600 psi
ASTM D790
285 MPa
41300 psi
ISO 178
Flexural Modulus 10.82 GPa
1569 ksi
ASTM D790
11.22 GPa
1627 ksi
ISO 178
Izod Impact, Notched 1.17 J/cm
2.19 ft-lb/in
ASTM D256
Izod Impact, Unnotched 10.35 J/cm
19.39 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 12.0 kJ/m²
5.71 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 70.0 kJ/m²
33.3 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 6.00 J
4.43 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 2.00 J
1.48 ft-lb
Multiaxial Impact; ISO 6603
Coefficient of Friction, Dynamic 0.59
0.59
ASTM D3702 Modified
Coefficient of Friction, Static 0.52
0.52
ASTM D3702 Modified
K (wear) Factor 36.3 x 10-8 mm³/N-M
18.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 263 °C
505 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
259 °C

@Thickness 3.20 mm
498 °F

@Thickness 0.126 in
unannealed; ASTM D648