Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.93 - 9.50 J/cm | 11.1 - 17.8 ft-lb/in | Average value: 6.63 J/cm Grade Count:13 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Izod Impact, Unnotched | 5.90 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
11.1 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH720 G30 30% Glass Fiber Reinforced PC Features:High mechanical strengthGood size stabilityLow tendency to warpGood surfaceSuitable for exact moldingApplications:Imaging equipment shellOA body frameElectrical equipmentComputer plug parts.. |
|||
Izod Impact, Unnotched | 5.90 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
11.1 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
Kingfa JH720 G50 50% Glass Fiber Reinforced PC Features:Excellent balance propertiesSuper high stiffnessHigh hardnessGood size stabilitySuper high mechanical strengthApplications:Imaging equipment shellOA body frameElectrical equipmentComputer p.. |
|||
Izod Impact, Unnotched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D256A |
LyondellBasell Higlass BJ44A Polypropylene Copolymer, 45% Glass Fiber Key Features: medium melt flow, high modulus, chemically coupled, glass fiber-reinforced polypropylene copolymer, high stiffness, good impact strength, excellent processabilityApplications: grille o.. |
|||
Izod Impact, Unnotched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP MFL36S PP LNP* LUBRICOMP* MFL36S is a compound based on Polypropylene resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Heat Stabilized, Wear Resistant. |
|||
Izod Impact, Unnotched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP MFL36S PP (Asia Pacific) LNP* Lubricomp* MFL36S is a compound based on Polypropylene resin containing Glass Fiber, PTFE. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched | 5.90 J/cm @Temperature 23.0 °C |
11.1 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp RL001 PA 66 LNP Lubricomp* RL001 is a Nylon 6/6 base resin containing PTFE lubricant. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers Amodel® AS-1566 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifica.. |
|||
Izod Impact, Unnotched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-651 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-651 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-651. This formulation offers some advantages relative to 30% carbon fiber reinforced PEEK which include better di.. |
|||
Izod Impact, Unnotched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D256 |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch.. |
|||
Izod Impact, Unnotched | 5.93 J/cm | 11.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DSL229 PC LNP* STAT-KON* DSL229 is a compound based on Polycarbonate resin containing 10% PTFE, 10% Stainless Steel. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Unnotched | 5.93 J/cm | 11.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DSL229 PC (Asia Pacific) LNP* Stat-kon* DSL229 is a compound based on Polycarbonate resin containing PTFE, Stainless Steel. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Izod Impact, Unnotched | 5.93 J/cm | 11.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Izod Impact, Unnotched | 5.93 J/cm | 11.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Asia Pacific) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Izod Impact, Unnotched | 5.93 J/cm | 11.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East) Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte.. |
|||
Izod Impact, Unnotched | 5.95 J/cm | 11.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON JX89626 PES LNP* STAT-KON* JX89626 is a compound based on Polyethersulfone containing Proprietary Fillers. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched | 5.93 J/cm | 11.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP 4X08423 FP-P (PFA) LNP* THERMOCOMP* 4X08423 is a compound based on PFA resin containing Glass Fiber. |
|||
Izod Impact, Unnotched | 5.93 J/cm | 11.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RF004XXH PA 66 LNP THERMOCOMP* RF004XXH is a compound based on Nylon 66 resin containing 20% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Izod Impact, Unnotched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics NORYL GFN3 PPE+HIPS (Asia Pacific) PPE+PS blend. 30% Glass reinforced.FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Suitable for fluid engineering applications including pump .. |
|||
Izod Impact, Unnotched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Izod Impact, Unnotched | 5.93 J/cm | 11.1 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Comtuf® 461 Glass Reinforced, Impact Modified, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Izod Impact, Unnotched | 5.90 J/cm | 11.1 ft-lb/in | ASTM D256 |
Adell RR-18 Copolymer Polypropylene, 40% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Izod Impact, Unnotched | 5.90 J/cm | 11.1 ft-lb/in | |
PBI Performance Products Celazole® PBI U-60 Unfilled Polybenzimidazole Resin U-60 grade Celazole® polybenzimidazole (PBI) resin is a organic polymer which does not burn in air and has high temperature resistance, along with excellent stability to chemicals and hydrolysis. .. |
|||
Izod Impact, Unnotched | 5.93 J/cm @Thickness 3.18 mm |
11.1 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® SPS-F-1006 HS Syndiotactic Polystyrene, Glass Fiber Reinforcement
(discontinued **) Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti.. |
|||
Izod Impact, Unnotched | 5.93 J/cm | 11.1 ft-lb/in | 73°F; ASTM D256 |
LyondellBasell Hostacom™ PF062-3 Polypropylene Homopolymer Description: Hostacom™ PF062-3 high melt flow, 5,200 MPa flexural modulus, chemically coupled, 30% glass fiber-reinforced polypropylene homopolymer has good impact strength, high stiffness and very.. |