Izod Impact, Unnotched 5.93 - 9.50 J/cm
11.1 - 17.8 ft-lb/in
Average value: 6.63 J/cm Grade Count:13
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor..