Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 14.2 J/cm @Temperature 23.0 °C |
26.6 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Stat-loy A3000Z ABS LNP* Stat-loy* A3000Z is a compound based on Acrylonitrile Butadiene Styrene resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for t.. |
|||
Izod Impact, Unnotched | 14.2 J/cm @Temperature 23.0 °C |
26.6 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |