Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 14.95 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 14.95 J/cm
28.01 ft-lb/in
ASTM D-4812
PlastiComp Complet® LGF50 - PA6 Nylon 6, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementInformation provided by PlastiComp, Inc..
Izod Impact, Unnotched 14.95 J/cm
28.01 ft-lb/in
ASTM D-4812
PlastiComp Complet® LGF50-PA12 Nylon 12, 50% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 12 with 50% long glass fiber reinforcementInformation provided by PlastiComp, In..
Izod Impact, Unnotched 14.95 J/cm
28.01 ft-lb/in
ASTM D-4812
PlastiComp Complet® LGF60 - PA6 Nylon 6, 60% Long Glass Fiber Reinforced
Complet® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 60% long glass reinforcementInformation provided by PlastiComp, Inc.
Izod Impact, Unnotched 14.95 J/cm
28.01 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Asia Pacific)
LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.
Izod Impact, Unnotched 14.95 J/cm
28.01 ft-lb/in
ASTM D-4812
PlastiComp Complet® LGF40 - PA66 Nylon 66, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 40% long glass fiber reinforcementInformation provided by PlastiComp, In..
Izod Impact, Unnotched 14.95 J/cm

@Temperature 23.0 °C
28.01 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Verton UX06451 PPA
LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 14.95 J/cm
28.01 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP VERTON UX06451 PPA (Europe-Africa-Middle East)
LNP* Verton* UX06451 is a compound based on Polyphthalamide resin containing Long Glass Fiber.