Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PlastiComp Complet® LGF50-PA12 Nylon 12, 50% Long Glass Fiber Reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, 50% Glass Fiber Filled
Manufacturer PlastiComp
Trade Name Complēt®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LGF50-PA12 Nylon 12, 50% Long Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 12 with 50% long glass fiber reinforcementInformation provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D-792
Filler Content 50 %
50 %
Long Glass Fiber
Mechanical Properties Metric English Comments
Tensile Strength 162 MPa
23500 psi
ASTM D-638
Elongation at Break 2.0 %
2.0 %
ASTM D-638
Tensile Modulus 11.724 GPa
1700.4 ksi
ASTM D-638
Flexural Strength 255 MPa
37000 psi
ASTM D-790
Flexural Modulus 8.276 GPa
1200 ksi
ASTM D-790
Izod Impact, Notched 4.27 J/cm
8.00 ft-lb/in
ASTM D-256
Izod Impact, Unnotched 14.95 J/cm
28.01 ft-lb/in
ASTM D-4812