Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 15.1 J/cm | 28.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Easy Molding, Internally Lubricated, Healthcare. |
|||
Izod Impact, Unnotched | 15.1 J/cm @Temperature 23.0 °C |
28.3 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp KI001A Acetal LNP* Lubricomp Fulton 441D is an Acetal based compound with Silicone.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 15.1 J/cm | 28.3 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP WX05505 PBT LNP* Thermocomp* WX05505 is a compound based on Thermoplastic Polyester (PBT) resin containing proprietary fillers. |