Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.88 J/cm @Temperature 23.0 °C |
16.6 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Thermocomp PH0700B PA 6 LNP* Thermocomp* PH0700B is a Nylon 6 base resin containing Tungsten. Characteristics are High Specific Gravity.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 8.84 J/cm | 16.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RC004SXS PA 66 LNP* THERMOCOMP* RC004SXS is a compound based on Nylon 66 containing 20% Carbon Fiber. Added feature of this grade includes: Heat Stabilized, Electrically Conductive. |
|||
Izod Impact, Unnotched | 8.86 J/cm | 16.6 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP VERTON UF-700-12 HS EXP PPA (Asia Pacific) LNP* Verton* UF-700-12 HS EXP is a compound based on Polyphthalamide resin containing Long Glass Fiber. Added features of this material include: Heat Stabilized. |