Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 99.99 J/cm - NB @Temperature -40.0 - -30.0 °C |
187.3 ft-lb/in - NB @Temperature -40.0 - -22.0 °F |
Grade Count:3 |
Overview of materials for Polycarbonate/PET Polyester Blend This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend". Each property range of values reported is minimum and maximum values.. |
|||
Izod Impact, Unnotched | 99.99 J/cm - NB @Temperature -30.0 - -30.0 °C |
187.3 ft-lb/in - NB @Temperature -22.0 - -22.0 °F |
Grade Count:13 |
Overview of materials for Polyetherimide (PEI) This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide". Each property range of values reported is minimum and maximum values of appropriate Mat.. |