Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.27 - 13.7 J/cm
8.00 - 25.7 ft-lb/in
Average value: 9.46 J/cm Grade Count:32
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..