Polymer Property : Izod Impact, Unnotched = 29.4 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 15.7 J/cm
29.4 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP ZI001 PPE+PS
LNP* LUBRICOMP ZI001 is a compound based on PPE+PS resin containing 2% Silicone. Added feature of this grade is: Wear Resistant.
Izod Impact, Unnotched 15.7 J/cm

@Temperature 23.0 °C
29.4 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubricomp ZI001 PPO
LNP* Lubricomp ZI001 is a compound based on Modified PPO containing Silicone. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region.