Mechanical Properties Metric English Comments
Izod Impact, Unnotched 3.63 J/cm
6.80 ft-lb/in
ASTM-D256
Ineos ABS Lustran® SAN DN79 SAN Grade
Lustran® SAN DN79 is a natural color, styrene-acrylonitrile copolymer supplied in pellet form. It is designed for used in compounding.
Izod Impact, Unnotched 3.63 J/cm
6.80 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES
LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing 30% Glass Fiber, 15% PTFE. Added featurs of this material is: Wear Resistant.
Izod Impact, Unnotched 3.63 J/cm
6.80 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP JFL36 PES (Asia Pacific)
LNP LUBRICOMP* JFL36 is a compound based on Polyethersulfone resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 3.63 J/cm
6.80 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP ZFL31XXC PPE+PS (Asia Pacific)
LNP* Lubricomp* ZFL31XXC is a compound based on PPE+PS Blend resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 3.63 J/cm
6.80 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66
LNP* STAT-KON* RE002 is a compound based on Nylon 66 resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 3.63 J/cm
6.80 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON RE002 PA 66 (Asia Pacific)
LNP* Stat-kon* RE002 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 3.63 J/cm
6.80 ft-lb/in
ASTM D256
Westlake Plastics Propylux® SD-X7 Polypropylene (static dissipative)
Low carbon black content (1-2%) reduces contamination problems from sloughing - clean room compatible. Also feature low leachable ion levels and low outgassing.Information provided by Westlake Plas..
Izod Impact, Unnotched 3.63 J/cm
6.80 ft-lb/in
ASTM D256
A. Schulman ComAlloy Aqualoy® 145 Polypropylene, Glass Reinforced, Chemically Coupled NSF
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced. In Aqualoy® materials, carefully selected base resins and proprietary additives meld hydrolytic stability an..
Izod Impact, Unnotched 3.63 J/cm
6.80 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 636 Nylon 6/6, Glass/Mineral Reinforced, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 3.63 J/cm

@Thickness 3.18 mm
6.80 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Lubricomp® JFL-4036 Polyethersulfone, Glass Fiber Reinforcement, PTFE Lubricant  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..