Polymer Property : Izod Impact, Unnotched = 3.90 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.08 - 5340 J/cm
3.90 - 10000 ft-lb/in
Average value: 7.33 J/cm Grade Count:55
Overview of materials for Polycarbonate, Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val..
Izod Impact, Unnotched 2.08 J/cm - NB
3.90 ft-lb/in - NB
Average value: 5.69 J/cm Grade Count:7
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a..
Izod Impact, Unnotched 2.08 - 4.43 J/cm
3.90 - 8.30 ft-lb/in
Average value: 2.97 J/cm Grade Count:13
Overview of materials for Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with Carbon Fiber + PTFE Filler". Each property range of values reported is ..
Izod Impact, Unnotched 2.08 J/cm

@Thickness 3.17 mm
3.90 ft-lb/in

@Thickness 0.125 in
ASTM D256
Fiberfil® PP-62/MI/25 Polypropylene Copolymer, 25% Mica Reinforced
Information provided by FIBERFIL Engineered Plastics
Izod Impact, Unnotched 2.08 J/cm
3.90 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer
LNP LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass, PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 2.08 J/cm
3.90 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON AX00756 ABS
LNP STAT-KON* AX00756 is a compound based on ABS resin containing Stainless Steel. Added feature of this material is: Electrically Conductive.
Izod Impact, Unnotched 2.08 J/cm
3.90 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RF006LXP PA 66 (Asia Pacific)
LNP* Thermocomp* RF006LXP is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Low Extractible.
Izod Impact, Unnotched 2.08 J/cm
3.90 ft-lb/in
ASTM D256
A. Schulman ComAlloy Comtuf® 101 Polypropylene, Mineral Reinforced, Impact Modified
Data provided by the manufacturer, ComAlloy International Company.25% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i..
Izod Impact, Unnotched 2.08 J/cm
3.90 ft-lb/in
ASTM D256
A. Schulman ComAlloy Voloy® 688 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod..