Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 21.3 J/cm | 39.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® LUX1619 PC Lexan* LUX1619 Polycarbonate resin is an extrusion grade. It is UL94 HB rated. It was designed for high light reflectance. |
|||
Izod Impact, Unnotched | 21.3 J/cm | 39.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® LUX2289 PC Lexan* LUX2289 resin is an injection molding grade with high light reflectance |
|||
Izod Impact, Unnotched | 21.3 J/cm | 39.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® LUX2619 PC Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance. |
|||
Izod Impact, Unnotched | 21.3 J/cm | 39.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Lexan® LUX2619 PC (Europe-Africa-Middle East) Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance. |