SABIC Innovative Plastics Lexan® LUX2619 PC

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Lexan®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Lexan® LUX2619 PC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lexan* LUX2619 Polycarbonate resin is an extrusion grade. It is UL94 V-2 rated at 1.5 mm. It was designed for high light reflectance.
Physical Properties Metric English Comments
Specific Gravity 1.34 g/cc
1.34 g/cc
ASTM D792
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Moisture Absorption 0.150 %
0.150 %
23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %
0.35 %
ISO 62
Linear Mold Shrinkage, Flow 0.0080 - 0.010 cm/cm

@Thickness 3.20 mm
0.0080 - 0.010 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 7.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
7.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
Type I, 50 mm/min; ASTM D638
Tensile Strength, Yield 57.0 MPa
8270 psi
Type I, 50 mm/min; ASTM D638
Elongation at Break 74 %
74 %
Type I, 50 mm/min; ASTM D638
Elongation at Yield 6.0 %
6.0 %
Type I, 50 mm/min; ASTM D638
Flexural Yield Strength 97.0 MPa
14100 psi
1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2.73 GPa
396 ksi
1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 6.40 J/cm
12.0 ft-lb/in
ASTM D256
1.35 J/cm

@Temperature -30.0 °C
2.53 ft-lb/in

@Temperature -22.0 °F
ASTM D256
Izod Impact, Unnotched 21.3 J/cm
39.9 ft-lb/in
ASTM D4812
Dart Drop, Total Energy 69.0 J

@Temperature 23.0 °C
50.9 ft-lb

@Temperature 73.4 °F
ASTM D3763
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 61.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
33.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
CTE, linear, Transverse to Flow 64.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
35.6 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
Deflection Temperature at 0.46 MPa (66 psi) 141 °C

@Thickness 3.20 mm
286 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C

@Thickness 3.20 mm
264 °F

@Thickness 0.126 in
unannealed; ASTM D648
Vicat Softening Point 147 °C
297 °F
Rate B/50; ASTM D1525
Flammability, UL94 V-2

@Thickness 1.50 mm
V-2

@Thickness 0.0591 in
UL 94
Glow Wire Test 850 °C
1560 °F
IEC 60695-2-13
875 °C
1610 °F
IEC 60695-2-13
960 °C

@Thickness 1.00 - 3.00 mm
1760 °F

@Thickness 0.0394 - 0.118 in
IEC 60695-2-12