Polymer Property : Izod Impact, Unnotched = 4.11 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.11 J/cm
7.70 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC
LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 10% PTFE/Silicone. Added features include: Electrically Conductive. Wear Resistant, Superior Molding.
Izod Impact, Unnotched 4.11 J/cm

@Temperature 23.0 °C
7.70 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp EB004 PEI
LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 4.11 J/cm

@Temperature 23.0 °C
7.70 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp EB004 PEI (Asia Pacific)
LNP* Thermocomp* EB004 is a compound based on Polyetherimide resin containing Glass Bead.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Unnotched 4.11 J/cm
7.70 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP UF006AS PPA
LNP THERMOCOMP* UF006AS is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized.
Izod Impact, Unnotched 4.11 J/cm
7.70 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DEP23FXC PC (Asia Pacific)
LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing Silicone, Carbon Fiber, PTFE. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 4.11 J/cm
7.70 ft-lb/in
ASTM D4812
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Izod Impact, Unnotched 4.11 J/cm
7.70 ft-lb/in
ASTM D4812
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Izod Impact, Unnotched 4.11 J/cm
7.70 ft-lb/in
ASTM D4812
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Izod Impact, Unnotched 4.11 J/cm
7.70 ft-lb/in
ASTM D4812
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Izod Impact, Unnotched 4.11 J/cm
7.70 ft-lb/in
ASTM D4812
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Izod Impact, Unnotched 4.11 J/cm
7.70 ft-lb/in
ASTM D4812
A. Schulman SCHULAMID® 66 GF13 13% Glass Fiber Reinforced Nylon 66
Information provided by A. Schulman.
Izod Impact, Unnotched 4.11 J/cm

@Thickness 3.18 mm
7.70 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Thermocomp® UF-1006 A HS Polyphthalamide, Glass Fiber Reinforcement  (discontinued **)
Features: Heat StabilizedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are sti..