Material Notes:
LNP STAT-KON* DEP23FXC is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 10% PTFE/Silicone. Added features include: Electrically Conductive. Wear Resistant, Superior Molding.
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
ISO 1183
1.29 g/cc
0.0466 lb/in³
ASTM D792
Moisture Absorption 0.120 %
0.120 %
50% RH, 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0016 cm/cm

@Time 86400 sec
0.0016 in/in

@Time 24.0 hour
ISO 294
0.0020 cm/cm

@Time 86400 sec
0.0020 in/in

@Time 24.0 hour
ASTM D955
Linear Mold Shrinkage, Transverse 0.0027 cm/cm

@Time 86400 sec
0.0027 in/in

@Time 24.0 hour
ISO 294
0.0030 cm/cm

@Time 86400 sec
0.0030 in/in

@Time 24.0 hour
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
ASTM D638
122 MPa
17700 psi
ISO 527
Elongation at Break 1.8 %
1.8 %
ISO 527
2.0 %
2.0 %
ASTM D638
Tensile Modulus 10.2 GPa
1480 ksi
1 mm/min; ISO 527
10.54 GPa
1529 ksi
50 mm/min; ASTM D638
Flexural Strength 186 MPa
27000 psi
ASTM D790
186 MPa
27000 psi
ISO 178
Flexural Modulus 9.10 GPa
1320 ksi
ASTM D790
10.3 GPa
1490 ksi
ISO 178
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Izod Impact, Unnotched 4.11 J/cm
7.70 ft-lb/in
ASTM D4812
Izod Impact, Notched (ISO) 7.00 kJ/m²
3.33 ft-lb/in²
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 27.0 kJ/m²
12.8 ft-lb/in²
80*10*4; ISO 180/1U
Dart Drop, Total Energy 16.0 J
11.8 ft-lb
Instrumented Impact Energy @ peak; ASTM D3763
Impact Test 3.00 J
2.21 ft-lb
Multiaxial Impact; ISO 6603
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 36.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.3 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
36.5 µm/m-°C

@Temperature -40.0 - 40.0 °C
20.3 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow 33.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.5 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
33.3 µm/m-°C

@Temperature -40.0 - 40.0 °C
18.5 µin/in-°F

@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 141 °C
286 °F
Flatw 80*10*4 sp=64mm; ISO 75/Bf
141 °C

@Thickness 3.20 mm
286 °F

@Thickness 0.126 in
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 137 °C
279 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
137 °C

@Thickness 3.20 mm
279 °F

@Thickness 0.126 in
unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
UL 94 by SABIC-IP
Electrical Properties Metric English Comments
Surface Resistance 10 - 1.00e+6 ohm
10 - 1.00e+6 ohm
ASTM D257
Users viewing this material also viewed the following: