Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.23 J/cm

@Temperature 23.0 °C
4.18 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp AF008 ABS
LNP* Thermocomp* AF008 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 2.23 J/cm

@Temperature 23.0 °C
4.18 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp AF008 ABS (Asia Pacific)
LNP* Thermocomp* AF008 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.