Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 4.40 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.40 J/cm
8.24 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® VX4910 ASA+PBT (Europe-Africa-Middle East)
10% Glass reinforced nucleated PBT/ASA with excellent mechanical properties high dimensional stability, and low density.
Izod Impact, Unnotched 4.40 J/cm
8.24 ft-lb/in
ASTM D256
ALM PA 606-FR Filled Nylon 12 Prototyping Polymer
Only commercially available fire retardant nylon 12 material, which meets FAR 25.853 60 second burn specification.The parts produced from PA 606-FR have a much smoother surface finish and sharper fe..
Izod Impact, Unnotched 4.40 J/cm
8.24 ft-lb/in
ASTM D256
ALM PA 650 Nylon 12 SLS Prototyping Polymer
Combines strength, durability (high impact) and chemical resistance and produces strong, durable, end use prototype parts. SL parts are less porous, more precise and have less noticeable build lines..