Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.65 J/cm

@Temperature -30.0 °C
4.96 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics Valox® SHF4930 PBT (Europe-Africa-Middle East)
Super high flow FR PBT grade with 15% Glass reinforced