Mechanical Properties Metric English Comments
Izod Impact, Unnotched 5.00 J/cm

@Temperature 23.0 °C
9.37 ft-lb/in

@Temperature 73.4 °F
ASTM D4812
DuPont Performance Polymers Rynite® RE5231 BK533 PET  (Unverified Data**)
Rynite® RE5231 BK533 is a 35% glass fiber/mica reinforced product modified for improved electrical properties such as dielectric strength.Information provided by DuPont Performance Polymers
Izod Impact, Unnotched 5.00 J/cm

@Temperature 23.0 °C
9.37 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics Cycoloy® EFX830ME PC (Asia Pacific)
Modified PC blend offering metallic look with minimal flow lines, flame retarded without using Chlorinated or Brominated additives.This data was supplied by SABIC-IP for the Asia Pacific region.
Izod Impact, Unnotched 5.00 J/cm
9.37 ft-lb/in
ASTM D4812
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East)
Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin.
Izod Impact, Unnotched 5.00 J/cm

@Temperature -30.0 °C
9.37 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics Valox® ENH4560 PBT (Europe-Africa-Middle East)
Valox* ENH4560 resin is a non-brominated/non-chlorinated flame retardant product based on Valox* PBT resin.
Izod Impact, Unnotched 5.00 J/cm
9.37 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP PDXE98480 PEI
LNP* Thermocomp* PDXE98480 is a compound based on Polyetherimide with Proprietary Fillers. Added feature of this grade: Reinforced.
Izod Impact, Unnotched 5.00 J/cm
9.37 ft-lb/in
ASTM D4812
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
Izod Impact, Unnotched 5.00 J/cm
9.37 ft-lb/in
ASTM D4812
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Asia Pacific)
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
Izod Impact, Unnotched 5.00 J/cm
9.37 ft-lb/in
ASTM D4812
SABIC Innovative Plastics NORYL NH8006 PPE+HIPS (Europe-Africa-Middle East)
Noryl* NH8006 resin is a 30% glass reinforced, modified PPE-PS blend. The material uses non-halogenated flame retardants to achieve a UL94 V0 flame rating (color specific) while offering an exceptio..
Izod Impact, Unnotched 5.00 J/cm
9.37 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP DC0041PQ PC
LNP* THERMOCOMP* DC0041PQ is a compound based on Polycarbonate resin containing Carbon Fiber. Added feature of this grade is: Flame Retardant.