Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 5.02 J/cm
9.40 ft-lb/in
Reliance Industries Polypropylene - 30% glass fiber filled
Information provided by Reliance Industries
Izod Impact, Unnotched 5.02 J/cm
9.40 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 121 Polypropylene, Glass Reinforced, Chemically Coupled
Data provided by the manufacturer, ComAlloy International Company.11% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.