Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 5.02 J/cm | 9.40 ft-lb/in | |
Reliance Industries Polypropylene - 30% glass fiber filled Information provided by Reliance Industries |
|||
Izod Impact, Unnotched | 5.02 J/cm | 9.40 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Hiloy® 121 Polypropylene, Glass Reinforced, Chemically Coupled Data provided by the manufacturer, ComAlloy International Company.11% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |