Polymer Property : Izod Impact, Unnotched = 5.69528 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.588399 - 3.04006 J/cm

@Temperature -30.0 - -20.0 °C
1.10231 - 5.69528 ft-lb/in

@Temperature -22.0 - -4.00 °F
Average value: 1.99 J/cm Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..
Izod Impact, Unnotched 0.588399 - 3.04006 J/cm

@Thickness 3.20 - 6.40 mm
1.10231 - 5.69528 ft-lb/in

@Thickness 0.126 - 0.252 in
Average value: 1.99 J/cm Grade Count:6
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is ..