Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.00 - 3.50 g/cc
0.0361 - 0.126 lb/in³
Average value: 1.08 g/cc Grade Count:174
Water Absorption 0.100 - 1.03 %
0.100 - 1.03 %
Average value: 0.488 % Grade Count:32
Moisture Absorption at Equilibrium 0.200 - 0.240 %
0.200 - 0.240 %
Average value: 0.206 % Grade Count:12
Water Absorption at Saturation 1.00 %
1.00 %
Average value: 1.00 % Grade Count:4
Maximum Moisture Content 0.0100
0.0100
Average value: 0.0100 Grade Count:13
Linear Mold Shrinkage 0.00100 - 0.0100 cm/cm
0.00100 - 0.0100 in/in
Average value: 0.00514 cm/cm Grade Count:131
Linear Mold Shrinkage, Transverse 0.00400 - 0.00900 cm/cm
0.00400 - 0.00900 in/in
Average value: 0.00550 cm/cm Grade Count:7
Melt Flow 0.100 - 42.0 g/10 min
0.100 - 42.0 g/10 min
Average value: 9.51 g/10 min Grade Count:177
Mechanical Properties Metric English Comments
Hardness, Rockwell M 102 - 103
102 - 103
Average value: 103 Grade Count:3
Hardness, Rockwell R 78.0 - 118
78.0 - 118
Average value: 104 Grade Count:114
Hardness, H358/30 80.0 - 98.0 MPa
11600 - 14200 psi
Average value: 86.5 MPa Grade Count:4
Ball Indentation Hardness 74.0 - 100 MPa
10700 - 14500 psi
Average value: 87.3 MPa Grade Count:6
Tensile Strength, Ultimate 24.0 - 138 MPa
3480 - 20000 psi
Average value: 40.4 MPa Grade Count:64
Tensile Strength, Yield 28.0 - 93.1 MPa
4060 - 13500 psi
Average value: 42.8 MPa Grade Count:146
19.0 - 63.0 MPa

@Temperature -40.0 - 80.0 °C
2760 - 9140 psi

@Temperature -40.0 - 176 °F
Average value: 41.0 MPa Grade Count:2
Elongation at Break 3.00 - 87.0 %
3.00 - 87.0 %
Average value: 23.7 % Grade Count:106
Elongation at Yield 2.00 - 10.0 %
2.00 - 10.0 %
Average value: 3.45 % Grade Count:57
2.40 - 3.60 %

@Temperature -40.0 - 80.0 °C
2.40 - 3.60 %

@Temperature -40.0 - 176 °F
Average value: 3.03 % Grade Count:2
Modulus of Elasticity 1.40 - 2.80 GPa
203 - 406 ksi
Average value: 2.10 GPa Grade Count:61
Flexural Yield Strength 47.1 - 579 MPa
6830 - 84000 psi
Average value: 73.4 MPa Grade Count:112
Flexural Modulus 0.210 - 13.1 GPa
30.5 - 1900 ksi
Average value: 2.42 GPa Grade Count:153
Izod Impact, Notched 0.220 - 5.88 J/cm
0.412 - 11.0 ft-lb/in
Average value: 2.91 J/cm Grade Count:145
0.550 - 3.80 J/cm

@Temperature -30.0 - 0.000 °C
1.03 - 7.12 ft-lb/in

@Temperature -22.0 - 32.0 °F
Average value: 1.52 J/cm Grade Count:11
0.48051 - 2.40255 J/cm

@Temperature -40.0 - 0.000 °C
0.90019 - 4.50096 ft-lb/in

@Temperature -40.0 - 32.0 °F
Average value: 1.52 J/cm Grade Count:10
0.48051 - 2.40255 J/cm

@Thickness 3.17 - 3.20 mm
0.90019 - 4.50096 ft-lb/in

@Thickness 0.125 - 0.126 in
Average value: 1.52 J/cm Grade Count:10
Izod Impact, Unnotched 3.25 - 5.07 J/cm
6.09 - 9.50 ft-lb/in
Average value: 4.28 J/cm Grade Count:4
0.588399 - 3.04006 J/cm

@Temperature -30.0 - -20.0 °C
1.10231 - 5.69528 ft-lb/in

@Temperature -22.0 - -4.00 °F
Average value: 1.99 J/cm Grade Count:6
0.588399 - 3.04006 J/cm

@Thickness 3.20 - 6.40 mm
1.10231 - 5.69528 ft-lb/in

@Thickness 0.126 - 0.252 in
Average value: 1.99 J/cm Grade Count:6
Izod Impact, Notched (ISO) 12.0 - 40.0 kJ/m²
5.71 - 19.0 ft-lb/in²
Average value: 25.2 kJ/m² Grade Count:34
8.00 - 18.0 kJ/m²

@Temperature -30.0 - -20.0 °C
3.81 - 8.57 ft-lb/in²

@Temperature -22.0 - -4.00 °F
Average value: 12.3 kJ/m² Grade Count:22
Izod Impact, Unnotched (ISO) 100 kJ/m² - NB
47.6 ft-lb/in² - NB
Average value: 100 kJ/m² Grade Count:10
80.0 - 100 kJ/m²

@Temperature -30.0 - -30.0 °C
38.1 - 47.6 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 95.7 kJ/m² Grade Count:7
Charpy Impact Unnotched 8.00 J/cm² - NB
38.1 ft-lb/in² - NB
Average value: 12.4 J/cm² Grade Count:30
7.00 J/cm² - NB

@Temperature -30.0 - -20.0 °C
33.3 ft-lb/in² - NB

@Temperature -22.0 - -4.00 °F
Average value: 10.3 J/cm² Grade Count:26
Charpy Impact, Notched 0.800 - 6.30 J/cm²
3.81 - 30.0 ft-lb/in²
Average value: 2.73 J/cm² Grade Count:42
0.500 - 3.00 J/cm²

@Temperature -30.0 - -30.0 °C
2.38 - 14.3 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 1.25 J/cm² Grade Count:29
Gardner Impact 10.6 - 31.1 J
7.82 - 22.9 ft-lb
Average value: 19.8 J Grade Count:4
4.00 - 4.00 J

@Temperature -29.0 - -29.0 °C
2.95 - 2.95 ft-lb

@Temperature -20.2 - -20.2 °F
Average value: 4.00 J Grade Count:1
Taber Abrasion, mg/1000 Cycles 68.0 - 93.0
68.0 - 93.0
Average value: 80.3 Grade Count:4
Thermal Properties Metric English Comments
CTE, linear 28.8 - 110 µm/m-°C
16.0 - 61.1 µin/in-°F
Average value: 85.4 µm/m-°C Grade Count:32
CTE, linear, Transverse to Flow 80.0 - 110 µm/m-°C
44.4 - 61.1 µin/in-°F
Average value: 89.3 µm/m-°C Grade Count:7
Thermal Conductivity 0.150 - 0.200 W/m-K
1.04 - 1.39 BTU-in/hr-ft²-°F
Average value: 0.190 W/m-K Grade Count:5
Hot Ball Pressure Test 95.0 - 100 °C
203 - 212 °F
Average value: 95.6 °C Grade Count:8
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+11 - 1.00e+17 ohm-cm
1.00e+11 - 1.00e+17 ohm-cm
Average value: 6.50e+15 ohm-cm Grade Count:36
Surface Resistance 1.00e+14 - 1.00e+15 ohm
1.00e+14 - 1.00e+15 ohm
Average value: 6.79e+14 ohm Grade Count:14
Dielectric Constant 2.60 - 3.10
2.60 - 3.10
Average value: 2.86 Grade Count:13
Dielectric Strength 7.00 - 48.0 kV/mm
178 - 1220 kV/in
Average value: 28.9 kV/mm Grade Count:34
Dissipation Factor 0.00480 - 0.0140
0.00480 - 0.0140
Average value: 0.00822 Grade Count:14
Arc Resistance 0.000 - 120 sec
0.000 - 120 sec
Average value: 80.0 sec Grade Count:6
Comparative Tracking Index 400 - 600 V
400 - 600 V
Average value: 590 V Grade Count:21
Hot Wire Ignition, HWI 7.00 - 120 sec
7.00 - 120 sec
Average value: 20.1 sec Grade Count:7
High Amp Arc Ignition, HAI 60.0 - 200 arcs
60.0 - 200 arcs
Average value: 122 arcs Grade Count:7
High Voltage Arc-Tracking Rate, HVTR 0.000 - 150 mm/min
0.000 - 5.91 in/min
Average value: 49.3 mm/min Grade Count:6