Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.94 J/cm | 14.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ4860HR PBT Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Izod Impact, Unnotched | 7.94 J/cm | 14.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Izod Impact, Unnotched | 7.94 J/cm | 14.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Europe-Africa-Middle East) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |