Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 7.95 J/cm @Temperature 23.0 °C |
14.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp DFI12E PC (Asia Pacific) LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli.. |
|||
Izod Impact, Unnotched | 7.95 J/cm @Temperature 23.0 °C |
14.9 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp DFI12E PC LNP* Lubricomp* DFI12E is a compound based on Polycarbonate resin containing Glass Fiber, Silicone. Added features of this material include: Internally Lubricated, Easy Molding.This data was suppli.. |
|||
Izod Impact, Unnotched | 7.93 J/cm | 14.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66 LNP* LUBRICOMP* RCL34 is a compound based on Nylon 66 containing 20% Carbon Fiber, 15% PTFE. Added features of this grade includes: Wear Resistant, Electrically Conductive. |
|||
Izod Impact, Unnotched | 7.94 J/cm | 14.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ4860HR PBT Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Izod Impact, Unnotched | 7.94 J/cm | 14.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Izod Impact, Unnotched | 7.94 J/cm | 14.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® IQ4860HR PBT (Europe-Africa-Middle East) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
Izod Impact, Unnotched | 7.93 J/cm | 14.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UX93847 PPA (Asia Pacific) LNP* Thermocomp* UX93847 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). |
|||
Izod Impact, Unnotched | 7.93 J/cm | 14.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP UX93847 PPA LNP* Thermocomp* UX93847 is a compound based on Polyphthalamide resin containing Proprietary Filler(s). |
|||
Izod Impact, Unnotched | 7.96 J/cm | 14.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOTUF PX06416 PA 6 LNP* Thermotuf* PX06416 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact. |
|||
Izod Impact, Unnotched | 7.96 J/cm | 14.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOTUF PX06416 PA 6 (Asia Pacific) LNP* Thermotuf* PX06416 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact. |