Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.75 J/cm | 8.90 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2210 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched | 4.75 J/cm | 8.90 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2210 PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched | 4.75 J/cm | 8.90 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2210F PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. |
|||
Izod Impact, Unnotched | 4.75 J/cm | 8.90 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2210K PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Izod Impact, Unnotched | 4.75 J/cm | 8.90 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2210K PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. |
|||
Izod Impact, Unnotched | 4.75 J/cm @Temperature 23.0 °C |
8.90 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Ultem 2210K PEI (Europe-Africa-Middle East) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched | 4.75 J/cm | 8.90 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2210R PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched | 4.75 J/cm | 8.90 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM 2210R PEI (Asia Pacific) 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing. |
|||
Izod Impact, Unnotched | 4.75 J/cm | 8.90 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics ULTEM HU2210 PEI 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP .. |
|||
Izod Impact, Unnotched | 4.75 J/cm | 8.90 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DEL36 PC LNP* STAT-KON* DEL36 is a compound based on Polycarbonate resin containing 30% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive, Wear Resistant. |
|||
Izod Impact, Unnotched | 4.75 J/cm | 8.90 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® VX5011 PBT (Europe-Africa-Middle East) VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics. |
|||
Izod Impact, Unnotched | 4.75 J/cm | 8.90 ft-lb/in | ASTM D256 |
A. Schulman ComAlloy Voloy® 441 Glass Reinforced, PET Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.32% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Izod Impact, Unnotched | 4.75 J/cm | 8.90 ft-lb/in | ASTM D256 |
LNP ULTEM® SMU5806 Polyetherimide, 8% Carbon Fiber Reinforcement
(discontinued **) Features: Low ShrinkageForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still.. |